Abstract
This review aims to provide a foundation for the safe and effective use of magnesium (Mg) alloys, including practical guidelines for the service use of Mg alloys in the atmosphere and/or in contact with aqueous solutions. This is to provide support for the rapidly increasing use of Mg in industrial applications, particularly in the automobile industry. These guidelines should be firmly based on a critical analysis of our knowledge of SCC based on (1) service experience, (2) laboratory testing and (3) understanding of the mechanism of SCC, as well as based on an understanding of the Mg corrosion mechanism.
| Original language | English |
|---|---|
| Journal | Advanced Engineering Materials |
| Volume | 7 |
| Issue number | 8 |
| Pages (from-to) | 659-693 |
| Number of pages | 35 |
| ISSN | 1438-1656 |
| DOIs | |
| Publication status | Published - 01.08.2005 |
| Externally published | Yes |
Research areas and keywords
- Engineering
ASJC Scopus Subject Areas
- Materials Science(all)
- Condensed Matter Physics
Fingerprint
Dive into the research topics of 'A critical review of the Stress Corrosion Cracking (SCC) of magnesium alloys'. Together they form a unique fingerprint.Cite this
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver